The problem is that dacron is used as peel ply in composite layups. Peel ply is used between the part being made and an absorber to suck up excess resin when vacuum bagged. Its used because the resin does not stick to it well so it can rip off after the part is done instead of being a lumpy mess. I also think it would be heavy.