RE: 1/12th Scale Edf Concorde
Ok Thomas, went to my local composites shop, they don't have the resin that you mentioned but theses are what they have and recommended for making these skins as structural part....
System 3 resin
MVS resin
Aeropoxy resins
Above 3 types comes with 3 speed hardeners "Fast, Medium and slow curing ones"
4th choice is "West Systems resin but due to it's thicker viscosity they didn't recommended that one for my applications.
Pint kits of above 3 types is between $45 and $55 bucks and Gallon is $140-$160 bucks
Obviously West systems gallon is far more expansive.
So what would you suggest as i think buying a gallon would be good way since fuselage will be double glassed also, both from outside and inside...