Assuming that it was a lacquer based primer, it most likely wasn't done "gassing off" when you applied the waterborne paint over it. The waterborne paint skinned over, trapping the evaporating solvents from the primer, creating blisters.

If you wait a week, or so, after priming, you could probably use the paint that you already have. Try it on a test piece. You have nothing to lose.