RCU Forums - View Single Post - Pipe diameter and wall thickness vs. turbine class
Old 11-22-2017 | 12:40 PM
  #8  
Dave Wilshere
 
Joined: Jun 2002
Posts: 13,258
Received 788 Likes on 571 Posts
From: Watford, UNITED KINGDOM
Default

Stainless oxidises less at high temperature, so less corrosion. There are different grades in the 300 range, the chromium content allows for the temperature tolerance above 500degrees

0.15 is more like it! Short pipe the weight penalty is low