Got the first mold halves done. The vortex mixer is really good at mixing in the high density filler.
Not difficult work but pretty intense.I will be doing my best to make these vacuum bag friendly.
I will leave these a couple of days to cure which will give me time to make the registration pins and sockets for the other side.
Last edited by RodneyFord; 04-07-2018 at 01:48 PM.