The best results at anealing are obtained if the metal is brought up to dull cherry red slowly so the part is heated the same temp right through, followed by slow cooling- easiest way to acheive slow cooling is to bury the hot object in builders lime( quicklime,white powdery lime) and leave till the next day or longer if a large peice.