RE: "Defective" Epoxy?
Try a couple more things before you throw it out. Mix a bigger batch. Epoxy cures with heat, the hardner generates heat. Smaller batches sometimes don't kick off completely. Second, mix up another batch and put it under the light. 2 hour epoxy should be tack free after a couple hours under a light, After is has cooled back to room temp.