Thanks Fellas for the info. I'll go with the epoxy as I used it to join the wing halves. It's a brand we get over here called Araldite, slow cure stuff. It's a bit thick to use so I got hold of some epoxy thinner called 91-92 from a local boat yard. I'll let ya's know how it goes. Hey Ed, would metholated spirits be denatured alchohol? Thanks again men. Regards John.