Fiberglass??
#2

My Feedback: (1)
Joined: Dec 2001
Posts: 3,759
Likes: 0
Received 0 Likes
on
0 Posts
From: Fort Wayne, IN
I went through the factory way back in 1982 and from what I remember, I think they used one layer of 1.5 or 2 oz and one layer of 6 oz with a polyester resin layup. They mixed cabacyl and polyester to fill the corners and details before the layup.